Stellite® alloy 25 is resistant to oxidation and carburization up to 1900°F. The alloy resists wet chlorine at ambient temperatures and is resistant to nitric and hydrochloric acids under certain conditions. Exposure testing is recommended to verify performance.
SPECIFICATION
- Specifications ASTM B435 / ASME SB435
- Width 1000mm / 1219mm /1250mm / 1500mm / 2000mm
- Length 2000 mm / 2440 mm / 2500 mm / 3000 mm / 6000 mm
- Thickness 0.1mm to 12 mm Thk
- Hardness Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.
Finish Hot rolled plate (HR), Cold rolled sheet (CR).
Form Coils, Foils, Rolls, Plain Sheet, Strip, Flats, Blank (Circle), Ring (Flange) etc. COBALT ALLOYS
Chemical composition
C % Si % Mn % P % S % Al % Cr % Cu % Ni % Mo % Nb % Ti % V %